Material | Polyester fiber/Polyester base fabric | |
Weight | g/m² | 450-600 |
Thickness | mm | 1.4-1.8 |
Finish treatment | Singeing, calendaring, shaping, flame retardant, waterproof, film coating | |
Air permeability | m3 / m2 / min | 13-16 |
Tensile strength | Warp | 1100 |
Weft | 1300 | |
Tensile elongation | Warp | 25 |
Weft | 50 | |
Temperature | ||
Continuos temperature | C° | 120 |
Instant temperature | C° | 150 |
Material | Polyester fiber/Polyester base fabric | |
Weight | g/m² | 450-600 |
Thickness | mm | 1.4-1.8 |
Finish treatment | Singeing, calendaring, shaping, flame retardant, waterproof, film coating | |
Air permeability | m3 / m2 / min | 13-16 |
Tensile strength | Warp | 1100 |
Weft | 1300 | |
Tensile elongation | Warp | 25 |
Weft | 50 | |
Temperature | ||
Continuos temperature | C° | 120 |
Instant temperature | C° | 150 |